TAKE ADVANTAGE OF OUR FREE SHIPPING TO US RESIDENTS!!!!!

From the makers of ALUMALOY as seen on TV we bring you Steelaloy is an easy to use, fluxless & arcless steel repair rod.  Also available Alumaloy, Castaloy, Copperaloy and Stainlessaloy

Just Imagine you can repair Steel using your own propane torch.  No Flux!  You can repair the thinnest to the thickest metal without warpage or distortion.  Steelaloy gives you the ability to repair motorcycle parts, bumpers, steel castings, oil pans, pipes, buildings, lawn mowers, tractor parts, fences, truck beds, radiators, rims, antiques and so much more. 

Strong permanent repairs that last a lifetime..

Aimetals is the first seller of Steelaloy on Ebay!  Don't be fooled by other listings that say Steelaloy as they could be inferior products.

Other Product Listings Available:
Castaloy, Alumaloy, Copperaloy & Stainlessaloy

Stock Description: 
You are bidding on 1 Pound of Steelaloy repair rods.  The rods are made in the USA. We will combine shipping on multiple orders. Shipping is free and customer satisfaction guaranteed.  Millions of Alumaloy rods have been sold throughout the world and Steelaloy is rapidly becoming just as successful!!!
 

Safety Instructions
Before use, the steel surface being repaired needs to be thoroughly cleaned with a fine wire brush. It is also important to always use a neutral flame and to keep the flame in motion. Always heat the surface being repaired and not the rod. Keep in mind larger objects may take longer to heat do to more surface area. Basic safety precautions are required and the proper safety gear such as gloves and eye protection should always be worn when working with this product. Loose clothing should never be worn when working with this product.


            

Physical Properties:

Temp range         400 deg f - 570 deg f
Compression Strength         60,000-75,000 psi
Tensile Strength        39,000 psi
Shear Strength           34,000 psi
Hardness ( Brinell-500 kg.load) :   100
Ductility        Good
Elongation     3% in 2 inches
Electrical Conductivity    24.9 (%IACS)
Thermal Conductivity     .24 cal/cm3/C
Corrosion Penetration     300 x 106 in 1 1/R
18-20 rods per lb 1/8" x 18"


          



 












Different types of repairs using Steelaloy

Butt Joints - Ends are beveled and brought together.  Follow tinning procedure, stroking both surfaces of the joint (with tinned groove) with Steelaloy.
Lap Joints – Parts can be tinned and slid together while rod is still molten, or a generous fillet of rod can be applied to the edges of the lap joint, making sure of tinning by running a stick through the molten area.
Mitered Joints – (in Windows, Doors, Screens& Frames) Material is solidly jigged.  A neutral flame is played over the joint area until Steelaloy will melt when drawn across the joint.  Make sure of tinning action by running solid end of rod through rod deposit. After tinning, the joint may be built up and finished as desired.  These joints are stable in the presence of humidity and have remained in perfect condition after many years of exposure.
Repair – (change design of steel, match patterns and dies) The section to be worked is cleaned by filing or grinding, then tinned by heating the aluminum to a temperature that will melt the rod when rubbed on.  When tinning, the Steelaloy rod should be kept out of the flame, letting the heat from the base metal melt the rod.  Build up with a soft flame.  Pre-heat the entire match plate of the die to approximately 600 degrees F facilitates the operation.
Weld – (white metal with Alumaloy) Clean plating or scale from surface to be welded.  “V” out fracture and set job up solidly.  Pre-heat generally with neutral or acetylene flame.  Just heat directly until parent metal starts to melt, then dip rod in and out of molten puddle to desired build up.
Stripped Threads – Drill old threads out over size so when new fillet is added all drilling and tapping will be done in Steelaloy.  This will make it easier to work with and will increase strength.  After drilling, heat base metal from bottom of hole up.  Tin rod into wall of hole beginning at bottom and work up.  Fill hole, cool, drill and tap as needed.
Notice: Discounts are available for large orders.  If you have lost your instructions or want to inquire about larger orders please contact us through ebay.  Thank you for your consideration of the Steelaloy product.

International Buyers – Please Note:

Import duties, taxes, and charges are not included in the item price or shipping cost. These charges are the buyer's responsibility.

Please check with your country's customs office to determine what these additional costs will be prior to bidding or buying..