Extremely High Precision Anycubic DLP printer built the same 3d model twice respectively with DLP Craftsman resin and general resin for comparison. When zooming in ten times to the surface of the model, we can see that the DLP Craftsman resin appears to have a smooth and exquisite surface, while general resin gets a blurred surface with obvious layer lines.
|
Fast Speed, Low Shrinkage Due to the upgraded formula, Anycubic DLP Craftsman Resin can improve the printing speed and lower the shrinkage rate of 3d models. The first exposure time can be as fast as 35 seconds, and the normal exposure time can be as fast as 2 seconds per layer. Molding shrinkage is as low as 3.7%.
|
|
ANYCUBIC UV Resin Series
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
ABS-Like Resin+ |
Water-Wash Resin | Basic Resin |
DLP Craftsman Resin |
UV Tough Resin |
Plant-Based Resin |
|
Features | High Strength, Excellent Toughness, Bending resistance | Easy to Wash, Easy to Shape, Low Odor, No Need Extra Alcohol Ideal for the Professional, High Toughness, High | Ideal for Beginners, Easy to Shape, High Rigid, High Precision | More Detailed, More Exquisite and Smooth, Low Shrinkage, Lighter Lamination | Ideal for the Professional, High Toughness, High Impact Resistance, Fast Curing | Plant-Based, Low Odor, Ideal for Beginners, Easy to Shape, High Rigid, High Precision |
Material |
UV resin |
UV resin + Hydrophilic polyurethane | UV resin |
UV resin + Ceramic powder |
UV resin | UV resin + Soybean oil |
Wavelength |
365-405 nm |
365-405 nm |
355-410 nm |
355-410 nm | 365-405nm | 355-410 nm |
Density |
1.05-1.25 g/cm³ |
1.15-1.20 g/cm³ | 1.05-1.25 g/cm³ |
1.05-1.25 g/cm³ |
1.10-1.15 g/cm³ |
1.05-1.25 g/cm³ |
Viscosity |
220-250 cP or mPa·s |
150-250 cP or mPa·s | 150-200 cP or mPa·s |
150-250 cP or mPa·s |
150-250 cP or mPa·s |
150-300 cP or mPa·s |
Molding shrinkage |
3.72-4.24 % | 3.72-4.24 % | 3.72-4.24 % | 3.72-4.24 % | 3.65-4.15 % | 3.72-4.24 % |
Surface hardness |
84 HD |
84 HD |
84 HD |
80 HD |
76 HD |
84 HD |
Flexural strength |
50-60 MPa |
50-60 MPa |
50-70 MPa |
59-70 MPa |
50-60 MPa |
59-70 MPa |
Tensile strength |
35-55 MPa |
30-45 MPa |
36-52 MPa |
36-52 MPa |
35-45 MPa |
36-52 MPa |
Flexural modulus |
1,400-1,600 MPa |
1,500-1,600 MPa | 1,200-1,600 MPa |
1.882-2.385 GPa |
800-1,200 MPa |
|
I-zod impact |
50-60J/m |
44-49 J/m | 50-60 J/m |
|||
Elongation at break |
20-30% | 8-15% | 11-20% | 11-20% | 30-50% | 11-20% |
1st-layer exposure |
20-40 s |
40-60 s |
20-80 s |
20-80 s |
60-80 s | |
Normal exposure |
1.5-2 s |
1.5-10 s |
3-15 s | 5-15 s (RGB) / 1-4 s (Mono) | 8-10 s | |
Heat deflection temp. |
60℃ / 140℉ | 60℃ / 140℉ | 60℃ / 140℉ | 60℃ / 140℉ | 80℃ / 176℉ | |
Resin wash |
Alcohol | Water/Alcohol | Alcohol | Alcohol | Alcohol | Alcohol |
Shelf life |
1.5 years |
1.5 years |
1 year |
1.5 years | 1.5 years |
1 year |