Technical characteristics of GKD1-500 / 20:
Filament voltage - from 6 V to 6.6 V.
The duration of the anode current pulse is not more than 30 μs.
The heating time of the cathode GKD1-500 / 20 is at least 5 minutes.
The heating time of the cathode in forced mode is at least 3 minutes.
The reverse voltage of the anode in a pulsed mode is not more than 20 kV.
The amplitude of the reverse voltage of the anode in the rectifying mode is not more than 16 kV.
The average current of the anode in a pulsed mode GKD1-500 / 20 - no more than 0.5 A.
The average current of the anode in the rectifying mode is not more than 2 A.
Anode current in a pulse - no more than 250 A.
Spark current - not more than 500 A.
The average current of the anode when sparking the load in a pulsed mode is 1 A.
The pulse repetition rate is not more than 5000 imp / s.
The minimum time between failures is at least 1000 hours.
The basic failure rate is 3.2 · 10-6 1 / h.
Gamma-percent resource GKD1-500 / 20 at γ = 90% - 1350 hours
The filling is hydrogen.
Design - cermet.
The cooling of the anode and cathode lead is forced, air.
The working position of the products GKD1-500 / 20 gas-cartridges - any.
It is allowed to supply the glow of the cathode and the hydrogen generator from one source.